Walnut tear-out
Bob S
Hi,
I noticed a divot / tear-out on a small tabletop I am making. In my shop, it had looked like it was just figuring in the wood until I got the right viewing angle. How can I fill / fix this prior to finishing??
Thanks,
Bob
Knowledge You Can Build On — Est. 1998
Walnut tear-out
Bob S
Hi,
I noticed a divot / tear-out on a small tabletop I am making. In my shop, it had looked like it was just figuring in the wood until I got the right viewing angle. How can I fill / fix this prior to finishing??
Thanks,
Bob
Re: Walnut tear-out
Don Stephan
Plane the area, sand the area, plane/sand the entire top thinner, inlay a walnut patch, wood filler and paint to match with fresco powders and shellac after first coat of finish are a few possibilities.
What size and depth?
Dick Coers
Because walnut will lighten with age, the filler/touch up color will show the entire life of the table. Well except for when you first match it. Do you plan on adding any stain of dye to the entire project? The more info you can give us, the more we can help.
Re: Walnut tear-out
Bob
You only get to do it once so make a new top. Something you can consider is routing a profile around the edge.
Re: Walnut tear-out
Pete in Holland, MI
Depending on how small, (corn kernel or smaller), in between coats of varnish, dribble enough varnish in the divot to fill it, let it dry and cure for several days, then sand over and continue layering up your varnish. It may need a second application to over-fill it prior to sanding/scraping smooth with the rest of the top. A clear filled in divot that you cannot feel may be better than splicing in a piece of wood that you may see over time.
Larger than a corn kernel, then you'll have to come up with a wood filler.
Yes, color changes over time will need to be considered in your selection.
Pete
Re: Walnut tear-out
John Pappas
I've had good luck filling in defects with small pieces of matching wood. The fit doesn't have to be perfect. Apply some glue, which will soften the replacement chip, then tap into place with a small hammer, or use clamps to press into place. Sand flush when dry. Try it on some scraps.
Re: Walnut tear-out
Jesse Cloud
Matching wood works well. Some tips:
look through your scraps for matching grain and color, ideally a cutoff from the same board. Doesn't have to be perfect.
Take a gouge and enlarge the hole slightly, making an oval hole.
With the same gouge, dig out a patch from the scrap, a little larger than the hole, may take a few tries to get it right, but its just scrap... Make sure the grain in the patch runs in the same direction as the grain from the hole.
When you get a nice fit, glue and clamp, sand flush later, then sand the whole piece. The patch will all but disappear. Wipe with a little thinner to reveal any leftover glue that needs sanding.
Re: Walnut tear-out
Bob S
Thanks for all the great ideas, I am glad I asked. The surface tearout is rather small (there are 2, each about 1/16 deep, 1/8 x 1/8. They were caused by the planer going over a board that had an area that was near a knot with no real grain. So, it is a very dark and very hard area. I think I will pursue filling the void rather than replacing or resurfacing the top, thanks for all the great options.
Bob
Re: Walnut tear-out
Don Stephan
If near a knot you might be able to fill with epoxy tinted black (I use black fresco powder) and have it look like natural variation in the wood around knots.