Home Articles Forums Gallery Marketplace Videos

WoodCentral Forums

Knowledge You Can Build On — Est. 1998

Compare cordless drills on the numbers that matter

cabinet/painting question

Posts

cabinet/painting question

#1

cabinet/painting question

Bruce, a MN Galoot

I'm about ready to paint a dresser/changing table I'm building for my son, DIL and first grandchild (drive-by gloat :D ). If this were to be stained and finished, I would sand to at least 220, maybe 320.

The question is, how finely does the surface need to be sanded for a surface painted with acrylic with a flow agent.

Thanks.

Re: cabinet/painting question

#2

First

Mark Mandell - Gone Round In New Jersey

Consider a sanding sealer. You haven't mentioned the kind of wood or your application method, but if you're using Flotrol, or similar, it would appear that you're spraying. Given that any wood will have it's grain raised with a waterborne/based finish, you'd do well to seal it first with a compatible sealer. 100 percent dewaxed shellac will do nicely, but there are other formulation out there. You may get a tad of grain-rise from the sealer that a light rub with 180 grit will take off and give your paint coating a good grip on the surface.

HTH

Re: cabinet/painting question

#3

Re: cabinet/painting question

Bill Tindall

I sand to 180, then spray with Kilz oil based thinned with mineral spirits. Then sand again with 180 and spray thinned oil based enamel. The result is glass smooth.

The Kilz is good at filling pores and the like, and it sands like chalk to a glass smooth surface.

Re: cabinet/painting question

#4

Re: cabinet/painting question

Bruce, a MN Galoot

What kind of sprayer do you guys use? An HVLP type?

Re: cabinet/painting question

#5

PS

Bill Tindall


Put it on wheels. This one as survived 2 generations and got asked for and retrieved from the shop for last granddaughter. Just got returned last week.(that daughter is optimistically done with diapers forever)

Re: cabinet/painting question

#6

Ancient DeVilbissJGA-502

Bill Tindall

Run at about 35-40 psi. must thin oil paints a bit (maybe 20-25%)

Re: cabinet/painting question

#7

More PS

Bill Tindall

the oil based Kilz isn't really oil based. It dries just a bit slower than lacquer. On a hot day I can spray the Kilz in the AM, sand in an hour or two , shoot the paint and it is dust free dry in a couple of hours (takes longer to harden of course) and it can be handled by mid afternoon or less.

Re: cabinet/painting question

#8

Re: More PS

Bill Tindall

there is water based Kilz, but I have no experience with it. the advantage of Kilz is that it is thick and builds a thick coat that can be sanded glass smooth.

Re: cabinet/painting question

#9

Re: First

Bruce, a MN Galoot

It's a maple frame with maple PureBond plywood panels. Poplar is used for secondary wood.

What sprayer do you use, Mark?

Re: cabinet/painting question

#10

Re: Shpraynzee

Mark Mandell - Gone Round In New Jersey

My main gun is a Walcom FX SP HVLP with a 2 qt. (CAT Bandit) pressure pot. For paint I change to a 1.9 tip and needle set and thin the product a bit more than with a bigger tip. I find I get more even atomization at lower pressures with that set-up. I think it also translates to better transfer efficiency and a more even coating, although the transfer rate is lower.

Re: cabinet/painting question

#11

Re: cabinet/painting question

Howard Acheson

Here is something that should help you in surface preparation.

Sanding wood--hard or soft--beyond 220 does little more than burnish the wood making staining difficult. This is particularly true if you are using a pigment stain which sits on the surface and relies on "nooks and crannies" to impart color. Softer more porous woods can be sanded to to 220 but harder less absorbent woods may stain best if only sanded to 150. The best compromise is to aim for 180 grit.

A number of years ago a large cabinet/custom furniture shop I was involved with did series of adhesion tests with various finishes and sealers. As part of this test we explored adhesion based on sanding grit. We found about the same adhesion up to 180 - 220. Beyond 220 adhesion dropped off due to burnishing of the underlying wood particularly when non-linear machine sanders were used. This was tested on birch panels. We also found that the resulting smoothness of the first coat of finish was not materially affected by the smoothnes of the underlying wood for sandpaper grits between 150 - 220.. The smoothest surface substrate for final finishes was obtained by sanding lightly after the first coat of finish was applied and dry. Which makes the case for a thinned first coat of finish.

So our conclusion was that sanding beyond 180-220 was not necessary and could be actually detrimental.

But, most important was that there was a big appearance affect if the surface was not HAND sanded in the direction of the grain using the highest grit used on the sanding machine. A flat pad sander produced a much flatter surface than a ROS. However, both required final hand sanding with the grain for optimum appearence. If not hand sanded, swirl scratches could show. Final hand sanding using a sanding pad in the direction of the grain is a must.

To carry it one step further, sanding at 320-400 grit after the first coat and subsequent coats was the optimum. No improved appearence was noticed by between coat sanding beyond 400 for varnish. 400 was the sweet spot for thinner finishes. Between coat sanding was always done by hand whether for flattening or for adhesion.

I think you will find similar thoughts in the popular finishing books but YMMV.

Finally, the first coat of ANY finish will soak little shards of wood and cause them to raise whether the surface was sanded, planed or scraped. When the first coat of finish dries these hardened shards are what causes the surface to feel rough. Sanding with 320 paper will remove these hardened shards and subsequent coats will go on smoother. So, smoothness counts after the first coat of finish, but not much before that.

The finish left by the sizing machine determines the starting grit. Jointers, planers, belt sanders etc, should leave a finish that allows starting with 100 grit. From there, go to 120 grit and sand until the marks from the prior grit are gone, then move to 150 and finish at 180 grit.

Plywood is factory sanded to 180 grit. Therefore, it's best to not sand plywood except with 180 grit and sand by hand. Get the first coat of finish on and then sand with 320. That way you are sanding the finish, not the wood. This avoids sanding through today's very thin surface veneer.

Re: cabinet/painting question

#12

That was interesting

Bill Tindall

All your conclusions from testing are exactly where I have wound up after years of finishing trials and errors. I never sand wood beyond 220 and always finish with hand sanding. If nothing else the hand sanding lets me intimately study the surface as I sand it. I sand the firist coat between 320 and 400, unless it is Paint (Kilz) which does well at 180.

Re: cabinet/painting question

#13

That's good to know, Howard,

Bruce, a MN Galoot

I don't usually sand wood above 220. I do like to use oil finishes, though, and apply the oil with 400 wet or dry sandpaper, and the resulting finish is smooth as my soon-to-be-born grandbaby's butt.

Re: cabinet/painting question

#14

Re: That was interesting

Howard Acheson

>>>> If nothing else the hand sanding lets me intimately study the surface as I sand it.

Valid Bill, and an excellent point. In my shop, the finishers did the final hand sanding in many cases. They were the ones charged with the final product inspection and we did not want a finger pointing exercise when there was something wrong with the finish.

Re: cabinet/painting question

#15

Re: That was interesting

Bruce, a MN Galoot

I remember from an interview with Thomas Moser in FWW way back in the early to mid-80's in which he said every one of his shop workers sanded every piece that came through the place.

Re: cabinet/painting question

#16

Bob

Re: More PS

Bob

Hi Bill, I do a lot of built in's like this one in the photo. I just sand to 220 grit then spray with water base primer, sand and tack, I apply 2 finish coats sand with 320 tack again and lay on a light coat of polly rub with 0000 steel wool, then wax. It cleans well don't peel or yellow and has lasted 5 years by just washing with mild soap and warm water.


img