finishing

ken chase

Before applying a water base lacquer to my project made of Koa I need

to bring out the grain. I don't like using danish oil and looking for a

good alternatate. Suggestions will be appreciated.

Thanks

Ken

Re: finishing

#2

Re: finishing

Mark Mandell - Gone Round In Jersey

Use a 1 lb cut of 100% dewaxed shellac. Apply two thin coats by spray is possible. For curly Koa I'd prefer either garnet or dark garnet, freshly mixed from dry flakes. Do not use any flow agents in the shellac mix as they tend to cause adhesion issues in waterborne top coats. Allow a good 48 to 72 hours for the alcohol to fully evaporate so it's not sitting there waiting to screw up your acrylic's tail solvents.

Re: finishing

#3

Re: finishing

Ken chase

Mark:

Thanks for the advise. What do you think of tung oil as an alternate choice?

Thanks again

Ken

Re: finishing

#4

Clint Searl

Re: finishing

Clint Searl

Anything that "wets" the wood, including your finish will emphasize the figure. A more pronounced effect can be achieved by staining with a pigment stain in a shade slightly darker than the wood's natural color, followed by sanding it back to leave the stain in just the more open pore areas. Then top coat.

Clint

Re: finishing

#5

Hope You're Not In A Hurry

Mark Mandell - Gone Round In Jersey

Expect several weeks for pure tung to cure up to the point of being topcoated. It is, perhaps one of the slowest curing oils we have. Using a tung oil finish like Waterlox would be faster, but you'll need to wait at least 7 days, preferable more. Reason here is that an oil needs a free source of oxygen to polymerize and link up. Top coat too soon and you'll wind up with a mess and maybe cracking because of the soft oil film that will be shrinking down towards the wood surface. Second, while I know people say they've done it, I do not recommend applying a waterborne finish directly over an oil surface. Thus I'd be applying a shellac tie coat anyway, which, by the way, will add a lot of depth to your finish film.

You can get the same "pop" of the wood's grain with a direct application of the shellac, and you won't have to wait except for getting the alcohol to evaporate.

My "standard" finish for cherry is to apply a coat of Waterlox sealer, let sit, apply 1-2 coats of dark garnet dewaxed shellac, let sit, then top coat with a waterborne finish. I'm obviously not in any hurry. :D Currently I'm using General Finish's Enduro Clear Poly with added cross-linker as a top coat . Very pleased with both the finish and its durability. Attached is an example on cherry:


and on ash over pigmented stain


Re: finishing

#6

Re: Hope You're Not In A Hurry

ken chase

I can't tell you how much I appreciate your suggestions and I plan to follow your advice about the

shellac. Thanks for taking the time to post the photo. You an nice guy!

Ken

Re: finishing

#7

Re: Hope You're Not In A Hurry

ken chase

Mark:

Had an idea I want to get you input on. My intent is to enrich the color of the koa

and I love the results I've been getting with waterbourne finish. What do you think of

adding a small amount of waterbase stain to my first coat and using clear on subsequent coats?

Your method is great but so far I've has difficulty finding the materials you suggested.

Thanks again for all the help

Ken

Re: finishing

#8

World of Difference *LINK*

Mark Mandell - Gone Round In Jersey

Between "stain" and "dye". If you put pigmented stain in your waterborne, you'll have mud. You can, however tint a waterborne finish with dye solution. In fact I use a number of TransTint [Homestead Finish - Jeff Jewitt] dyes to push finishes one way or the other. I do so only in the shellac coat, keeping the top coats "pure."

If you want to tint your finishes, I strongly suggest that you put in some serious application practice. Hand-applying a tinted finish is seldom done because of the lap-marks that show up. Successfully spraying a tinted film takes a very light and even touch with a good gun to avoid splotches, although some variation in the color can give interesting results. This is also why I tint the shellac. If I screw it up (happens!) it comes off with an alcohol rub-down. Mess up on a tinted waterborne coat and you're sanding and stripping the whole piece, to start over.

Example: I had a devil of a time getting a finish combination to match the existing pieces next to that ash trestle coffee table. So I put down the base stain, sealed it with ultra pale shellac, then misted on a very light haze of tinted shellac. Match was almost perfect. I then put my pure waterborne on, and except for the sheen, you can't tell them apart. BTW, the cherry was leveled and rubbed out to gloss; the coffee table was left "off-the-gun" with a very slight orange-peel surface that has done beautifully for wear resistance.

As far as sourcing, I'm attaching a link to Jeff Jewitt's site. From shellac to top coats to colorants and application tools, he's got it all and his books are outstanding. You can call him for direct advice as I do.