Anyone use Penofin finish

BradinMD

I'm interested in other's experience using Penofin finishes (the Blue or Red) on outdoor projects. I have a douglas fir screen door I'm building and was considering Penofin vs. Waterlox Marine finish. From what I read, the Penofin does not build a finish and would look natural. The Waterlox Marine would not build a finish but is high gloss. Anyone have experience with this products?

Re: Anyone use Penofin finish

#2

Re:Penofin finish

Mark Mandell - Gone Round In Jersey

I use Red Label Penofin on my decks. It is less a finish and more a treatment. Goes on easily, however you must wipe it off well in accord with the directions or it will form a gummy surface that's a pain to wash off. Ellis can contribute to how my 20 year old decking looks. I expect to reapply to horizontal surfaces every 2 years; verticals should "last" for 4.

Seems to be doing well on the decking with no mildew in the full shade sections. The application to large ares is a pain, however, because you really have to carefully wipe it dry within about 20 minutes (think lots of towels that you'll throw away). Lap marks are not a problem, but do not apply in full sun.

hth

Re: Anyone use Penofin finish

#3

Re:Penofin finish

Doug Reynolds in Seattle

I too use the higher rating of Penofin on my Ipe deck and am very happy with it but, you must follow the directions of wiping off, no direct sunlight and wood must be and stay dry for at least 24 hours. I reapply every two or so years when I remember. Penofin and Sikkens (sp?) is supposed to be the best for such applications.

Re: Anyone use Penofin finish

#4

I've used both...

John in NM

And as far as I remember, the Waterlox is indeed a film finish. Not sure how they could make a glossy non-film :D.... Its a bit thinner than "spar" varnishes like McCloskey's but still a bit thick and sticky for wipe on application if you're used to the sealer-finish.

Penofin is about equivalent to Sikkens on Ipe decking, should work fine on fir, I don't think you'll have the wiping off quick enough problem since a door is small and fir should soak it right up, leaving none to wipe! Both Penofin and Sikkens SRD have lasted on the order of 6 months for me - but I'm up at 7000' where we get a ton of finish destroying UV.