Waterlox application question

Vincent Booth

Has anybody used Waterlox Original Finish without first applying the Sealer/Finish? Is it necessary?

I already have one gallon of the Original Finish for my just under 500 sq ft floor but do not have the Sealer/Finish.

Is one coat of the Original Finish going to properly protect the floor or should I order the Sealer?Finish and wait for it to arrive?

If it matters, the floor is heavily stained white oak.

Re: Waterlox application question

#2

Clint Searl

Re: Waterlox application question

Clint Searl

Check out the Waterlox website for instruction videos.

Clint

Re: Waterlox application question

#3

Re: Waterlox application question

Howard Acheson

In reality, the Waterlox Original Sealer/Finish is just an intermediate sheen between their Original Gloss and their Satin. Here is something published by Waterlox on another forum.

QUOTE

Just to clarify a couple of items noted here regarding Waterlox Finishes.

If you would like a medium sheen, use the Sealer/Finish for all coats required. (3-4 depending upon if it a hard wood or a soft wood. Additional coats may be desired if wiping the varnish.) Our Original Sealer/Finish is the only finish in our line that mellows with age. It will start off at about a 75 degree gloss level the day it's finished; and will fade to a 50-55 degree gloss in 4-6 months.

If a lower sheen is desired, the last coat applied should be our Waterlox Original Satin Finish. Using our Original Satin Finish will produce a gloss level of about 20-25 degrees.

If a higher gloss is desired the last coat applied should be our Waterlox Original High Gloss Finish. Our Original High Gloss Finish will produce a finish that has about an 85 degree gloss level.

With the exception of our Marine Finish, there is no diference in the durability of the finish regardless of which product is used. All are equally suitible as a finish/top coat, it simply depends on the gloss level that is chosen.

For example, our Original Satin Finish is our Original Sealer/Finish with a flattening agent (pigment) added to cut the gloss level. The Original High Gloss Finish is our Original Sealer Finish with an additional resin to increase the gloss level.

We do not add a UV inhibitor to our finishes. Direct UV light will break down any finish over time. Our Waterlox Original Marine finishing system is formulated as a traditional Tung oil spar varnish. It is made from Tung oil and a special resin mixture that forms a protective and elastic finish against sun and salt/fresh water exposure. Our Waterlox Original Marine Finish when used as a finishing system in conjunction with Waterlox Original Marine Sealer penetrates and waterproofs and reflects the UV instead of absorbing it.

When the gloss begins to fade, this is the key to knowing that the UV rays are beginning to affect the finish and that it�s time to re-coat. Sanding down to bare wood is not necessary to refinish the surface, simply clean the surface and apply another coat of Waterlox Original Marine Finish (view our product bulletin). Keep in mind however, that if proper maintenance is not followed, and the finish is left to degrade too long, the film can peel. This is due to the film shrinkage from the UV light.

Hope this helps.

Chip Schaffner - Waterlox Coatings