Why glue joints fail
Bill Tindall
It was shown below that excessive clamping pressure in NOT a cause of failed glue joints. So, what is the cause? Glue works by "wetting" the surfaces to be joined. It follows that both surfaces must be wetted for the bond to form. A common cause of a wetting failure is allowing the surface of the glue to dry some before assembling the joint. This kind of failure can result when glue is applied to only one side of the joint. Any drying will hinder transfer and wetting of the mating wood surface.
A second problem resulting from letting glue dry too much before assembly is a thick glue line. As the glue dries its viscosity increases dramatically. If the viscosity is too high before clamping then the excess glue will not be squooze (E. TN word) from the joint and a thick glue line will result.
Another source of failure is the result of gaps. The strength of the glue dried in a gap is less than that of the wood so a thick glue line will result in fracture through the weaker glue rather than the stronger wood. It takes but the tiniest thickness of glue to form the strongest possible joint. Any amount of glue in the joint greater than this optimum thickness will therefore weaken the joint. Perhaps gapping joints beget excessive clamping pressure to try to close them and that is the source of the clamp pressure myth.