Alkyd paint question
Nathan
For a project I'm working on I decided to use alkyd paint. I'm rolling it on with a roller. First I put a coat of primer on and, being distracted by other stuff, let it dry for a long time. It sanded quite well. I hand sanded to 240-grit and the surface felt very smooth.
Now, 24 hours ago I put the first finish coat on, again using the roller. I was pleased with how it turned out but it needs more (wood grain is visible) probably two coats more. The surface looks nice (like an egg-shell, as advertised) but is a bit rough to the touch and I don't want the roughness to get any worse as I apply more coats.
I tried sanding with 240-grit but it quickly gummed up the sandpaper and I did not get the really smooth surface like before on the primer.
I'm assuming this is because it's only been curing for 24 hours and the temperature in the shop is fairly cool, arout 55 degrees, so the paint is not yet completely cured. Is this assumption correct, do you think? Also, is sanding between the finish coats the right thing to do, and what grit or grits would you use?
Thanks as always for any advice you can provide. Even if it's not about alkyd paint in particular, any general advice would be appreciated as I am a beginner.