Removing end grain dent

Dan Mitchell

>I accidentally knocked a leg for a table I'm making onto the concrete shop floor & dented the end grain at the top of the leg.

And NATURALLY, the corner that smacked the floor just COULDN'T have been the INNER one which wouldn't show so it wouldn't have MATTERED.

NOOOOOO, of COURSE NOT!!!!

;-)

So anyway, the wood is hard maple, the leg is 1.75" square at the top where it is dented. I'd say at the maximum, the wood is pushed down a little over 1/16. I've seen people "steam" wood dents back into something resembling the original appearance, using an iron, anyone have any particular tips on doing this with an end-grain injury?

TIA

Dan


img

Re: Removing end grain dent

#2

Re: Removing end grain dent

Dick Coers

>I've used a clothes iron and wet rag many times. It may take several "hits" (pun intended) with the process, but since no grain is broken you should have good luck. I would just put a little water on the maple first, then put a wet rag on the face grain of the dent, then bring in the iron. You will have to angle the iron so it directly contacts that dented area. I would mostly stay off the end grain, but a pass or two with the rag and iron can't hurt. To help dry off any moisture on the surface, I usually take the bare iron over the wood for a couple quick passes. Don't hesitate because you don't want to scrape off burnt wood too.

Re: Removing end grain dent

#3

Just chamfer it

Alexander Grigoriev

>

Re: Removing end grain dent

#4

Re: Just chamfer it

jan derr

>if the piece is heirloom why worry?

correcting or not correcting mistakes is hand made in america.

Re: Removing end grain dent

#5

Re: Just chamfer it

Fred Davis

>The Pic looks like more depression then steaming will bring back , so if it don't, consider trimming all four to a new length

FredD

Re: Removing end grain dent

#6

Re: Just chamfer it

Barry Irby

>A 1/16"? Take a whack at swelling it back up and if that does not work just trim all four legs enough to eliminate it.

Re: Removing end grain dent

#7

put in a Dutchman

paul in AZ------WebKitFormBoundary+isMX5X2paiDYC5e

>Carefully cut out the dent in a triangular fashion and make it a little deeper, as much as a quarter inch deep, then glue in an insert.

You should be able to find a good grain match in the cutoff scraps of wood.

Not hard to do and nobody will ever notice the repair.

Re: Removing end grain dent

#8

Before trying anything drastic

Lee Schierer - McKean, PA

>What I would try first is to place one or two drops of water directly on the dent. Walk away for an hour or two and see what happens. My bet is the wood will swell back up to the original size. It might require a second appliation of two drops of water to complete the job.

Lee

Re: Removing end grain dent

#9

Re: Removing end grain dent

Tony - Memphis

>I have had real good luck steaming. 1/16" is a bit much to ask, but I would try it. I wet the wood good, then place a wet piece of cotton tshirt material over it and hit with the iron on high. I just did this on some curly maple table skirts a few nights ago. I think I had them a little loose in the vise when I was trimming the tennons and I got a nice dent in the shape of the corner of my vice cheek in them. Came right out. The other option is to trim the corner along the lines of the grain and glue a new piece on and then trim it down. I saw this in an article (Phil Lowe in FWW?). Nice trick for corners and it works well. Good luck with it. I feel your pain! Been there many times.

Tony

Re: Removing end grain dent

#10

I just fixed this same problem

Bill Tindall, E.TN

>I was showing daughter her table leg and it fell over and made an identical dent. It steamed out nicely. Soldering iron+ wet rag- apply wet rag to dent and soldering iron to rag so as to make quantities of steam. repeat until dent is largely gone.

Now, wait a while until the water added goes away before sanding back smooth, or I keep a hair dryer on hand for drying these fixes so I can get on with finishing.

How it works: The steam plasticizes the cellulose and makes it capable of swelling. The steam swells the compressed wood cells. Dents that have not torn fibers will typically steam back to original condition.

Re: Removing end grain dent

#11

Re: Removing end grain dent

Dan Mitchell

>I made a "gutter" around the top of the leg with wide packaging tape, clamped the leg in the vice such that the dinged area was angled down, & put a few drops of water in the gutter, immersing the ding. Let this sit about an hour, then applied the iron to the edges around the saturated ding, as well as heating them through a damp towel. After 2 such treatments, I'd say the area is about 90% of what it had been prior to the dent, which is fine for this application.

I couldn't just easily shorten all the legs, since I'd already cut the mortises & made the tenons on the apron bits, plus cut the sides for a drawer that will be included.

Thanks for the tips.