Electrolysis Improvement
Tom MacGregor
>Since electrolysis used to derust tools tends to be "line of sight" I wondered if it was possible to improve the line. I picked up a salvageable V&B 907C on ebay and wanted to dunk the whole body at once, not my usual flip-it-in-the-bucket routine. I bought a cheap (under $5) plastic trough for soaking wallpaper long enough to immerse an object up to 30 inches long. A short chunk of sacrificial iron concentrated the rust removal on less than 1/4 of the plane body. I took a 5-1/2 foot long piece of 1/4 inch iron rod and bent it into a long U around the trough and hooked it up as shown below. I got bubbles the full length of both sides of the plane! I will note, however, that it's very easy to make a BIG mess if you're not careful dumping the liquid out of the trough. Please DAMHIKT.