>Just picked up a beautiful piece of S4S 4/4 cherry from the lumberyard this afternoon and I'm wondering how long before I can work with it. Basement shop. Kinda chilly down here but not too cold to cut some wood.
>It's not the shop you need to be concerned with, but the resulting location. A cool moist basement shop is different than a warm dry heated living room.
>Acclimating (or acclimatizing) wood is usually done to either allow the moisture content to stabilize at a different level or to allow the moisture to disperse more within the board itself. This minimizes unwanted shrinkage, distortion (cup, bow, twist) and/or reaction during and after construction. But your wood doesn't necessarily need to be acclimatized if the moisture distribution is uniform and the moisture content is within a usable range for your project. So, what you need to know is the current moisture content and the "destination" moisture content (my term for the final MC of the piece in its intended surroundings). It helps to have a moisture meter, although you can determine moisture content with an accurate scale and an oven. I won't get into that now, but it has been explained many times in our archived messages.
The destination moisture content, as Pete pointed out, is the most important determining factor. If the finished piece will live in your house, you can take moisture readings on furniture that you already have in the intended location. The difference between the MC of these pieces and your lumber will tell you what to expect in the way of shrinkage or expansion by the time your lumber reaches equilibrium with your home environment. Realistically, assuming you've designed your piece using correct design principles, shrinkage should not be much of a factor except for critical elements like wide door panels which could shrink out of their grooves if the wood is too wet, or blow the frame apart if it is too dry. In those cases, you need to design the joinery and dimensions to accommodate the expected wood movement. shrinkage is more of a factor with applications like flooring, where large gaps will open up if the wood is not properly dried in advance.
The bigger issue v. acclimatizing wood is getting all the stresses out of the lumber. If it was kiln dried and then sat on somebody's warehouse rack or in a boxcar and absorbed moisture on the outside, it will have a gradient of moisture through the board. Stacking it with good ventilation for a while will allow those stresses to relax. This will help assure that when you joint the board flat, it will stay flat, and when you tablesaw it, the kerf will not clamp shut on your blade, or when you resaw it, the pieces will not cup all over the place. You can check the gradient by taking moisture readings at different depths in the wood.
There's yet another aspect to all of this, and that is that, depending on the joinery and the design of your piece, moisture content might not matter at all. For centuries, carpenters made furniture from green wood and let it shrink as it dried. They still do in many parts of the world. As long as the design doesn't have any points where shrinkage will result in self-destruction, you can get away with it, although there will still be other issues, such as finish adhesion, etc. I'm just mentioning this so you understand that there are many variables to furniture design.
>The presumption is that this lumber yard sells to commercial customers.
Commercial customers don't typically inventory much lumber. Ours called in an order and they were working it soon after delivery. The conclusion is that commercial shops can successfully build stuff from this lumber without further ado or at least that should be the case with a reliable lumber source.
If you had an acclimation issue the answer to your question is indeterminate. How long it takes lumber to go form moisture content A to B depends on many factors- temperature, air flow, wood species and thickness, etc.
The bottom line is that either you can work this lumber at once, or you need some means of following its moisture content to know when it is right for your purposes.
>Wow! There's a lot more to this than I thought. Thanks for the detailed response. You hit the mark with the part about stress. That is my main concern. This piece of wood is so beautiful I'd hate to see it split and warp on me. I'll let it sit in the shop for a while and maybe Santa will bring me a moisture meter for Christmas. Thanks again.
>I have to disagree with Ellis on the wood stress theory. If the lumber has stress in it, it is vastly more likely to be a result of improper drying to begin with and NO amount of acclimation on your part will fix the problem. Only resteaming the lumber will relax it.
I do agree that if the lumber is wet and you lay one side on the bench in a dry shop the exposed side will dry and cut up. But if your saw stalls while ripping, or the boards spread upon ripping or resawing, this is an initial drying induced stress problem, which, as I said earlier, is not fixable by you.
Cherry is one of the easiest woods to dry so I would not expect there to be drying problems. Furthermore, I see mills being more picky about drying than they used to be, probably in response to more demanding export market. In addition, the hardwood market has tanked so operations are not rushing kiln charges out the door to meet an expanding demand.
Instead of fretting about whether the lumber is ready to use, worry about whether you are ready to use it. Have you acquired the skills on cheaper wood to be able to successfully make what ever you intend to with this cherry?
>Ellis makes some valid points and so does Pete and Bill , but none covers all of the issues with stressed lumber.
Case hardening and reverse Case hardening is caused by incompetent Dry Kiln operators and once the lumber is out in the market away from the Kiln so it cannot be fixed with steam , there is nothing you can do about it as Bill says .
Another frequent source of Stress and Strain not mentioned is Tension and Compression grain caused by a tree leaning while growing.
Ripping this type of lumber can cause more excitement then you may have anticipated.
Acclimation as Ellis points out produces the best possible approach to use of the lumber.
Any competent and knowlegdable flooring contractor will store the hardwood flooring in the area it is intended for a week or so in advance of laying it for that reason.
Moisture content is always the most important factor to consider when building a piece and what I done over the years to minimize this problem is let the lumber which supposedly is KD to start with , but may be as high as 14-15 percent because the mill operator stores it in buildings open at both ends, stay in my shop until it is as dry as the shop environment which runs under 6 % MC for the lumber I store in it.
This permits me to build with the knowledge the the lumber will only expand , if it moves any at, in the place where it will reside and never have the problem of shrinking and opening the joints.
It is far easier for me to predict the outcome , if I approach the piece with bone dry lumber.
Buy a moisture meter , you will be amazed at what it will tell you.
>... Bill, my suggestion was that if the board was cupped or stressed because of absorbing or giving off moisture after drying, it could be brought back to equilibrium by letting it sit for a while. If it was improperly dried, I agree, you won't be able to relax it without steaming it.