useless Folklore
Bill Tindall, E.TN
>I wish this 1year/in folklore would die a timely death.
The drying rate of lumber is influenced by species, thickness, air circulation, temperature, humidity and probably some other variables I haven't thought of. Without knowing these conditions it is impossible to estimate a rate as it could vary by an order of magnitude. As an example, under controlled conditions 4/4 poplar can be dried from the saw to 7% MC in less than a week while for oak the time is at least 30 days. On the other hand In most outdoor environments lumber will never get to 7%, if that is your target. You don't want to dry 3" lumber at the same rate as 1" or stress will be induced.
But to answer your specific question, the time to get to a target moisture content under some specified condition will be dependent on surface to volume ratio, and some surfaces dry at a greater rate than others. However, in a practical situation this variable is insignificant compared to the variables enumerated above. I have never heard of a kiln drying 4/4- 8 foot lumber any different than 12 foot lumber, for example. In fact, a variety of lengths are typically loaded into a kiln at the same time, but the thickness will be the same.