Re: Aniline dye
Sgian Dubh
>Water based aniline dye won't remain wet on the surface long enough to cause the PVA glue to soften to the point of loosening its grip.
You'd also need to ensure the dye you have is soluble in either water or alcohol. If it was sold to you and labelled as water soluble it's not soluble in other solvents.
There is another factor to consider: water based dyes give the finisher more time to work them onto the surface because of their longer drying time, and make it easier to avoid 'tide marks' which spirit (alcohol) based dyes are prone to if applied carelessly.
If you do use water based dye you first need to get a cotton cloth well dampened with clear, warm or hot water and work this over the surface with the grain. This raises the grain. Let the surface dry and lightly sand the surface smooth with a bit of 220 or 240 grit abrasive paper. Then apply your dye. This way you've already done the grain raising that water based dye applied without the preliminary grain raising stage would cause. It leads to a much smoother surface ready for your polish. Slainte.