David Best

>I have made a hall bench for my son and his family, from quarter sawn oak and black walnut,because of the wear and tear of 3 grandchildren and 4 dogs, I decided to use varathane water based floor finish.

The nibs that have been raised is unbelievable, it's almost like rough sawn lumber, I did sand it down to 400,because I wasn't using any stain,fortunately I have only done the underside so far , but it is harder than nails to sand back down.

Any suggestions on what I should do for the top side, I have until Feb 13th to get it finished.

Thank you for any help.

David

Re: finishing question

#2

Re: Beating the Fuzz

Mark Mandell - Gone Round In Jersey

>David,

Putting any waterbased finish on raw wood will raise the grain as you've found out. You can minimize this effect by raising the grain first with water, then very lightly sanding off the fuzzies when dry.

Better yet is to prevent the fuzz by using a coat of sanding sealer or dewaxed shellac before applying your finish. There are both solvent based and waterborne sanding sealers that work well, or it's easy to pad on 2 light coats of Zinsser's SealCoat cut 50/50 with denatured alcohol. Lightly sand in the direction of the grain, vac off (no tac cloths here), then apply finish.

Good luck

mm

Re: finishing question

#3

Re: finishing question

Bill Tindall, E.TN

>Oak only needs to be sanded to 180 before first coat.

After first coat I sand with 320 stearated paper (has the white powder on it to lessens loading problem). For a floor I would use 220. The 220 can leave visible scratches in the finish. You could use 0 steel wool but it will be slower. Then recoat once or twice.

If you want glass smooth, after the last coat you could sand again with something in the range of 320-400 and then rub out with 4/0 steel wool and wax.

Re: finishing question

#4

Re: finishing problems

Mark Mandell - Gone Round In Jersey

>Bill, if he uses stearated paper with his waterbased finish he'll have a mess with the finish fisheyes and peeling off. Likewise, under or during waterbased finishing, using steel wool will put oil on the surface and imbed steel fibers in the pores which will rust in the finish.

From your response, I'm thinking one of us misread the question.

mm

Re: finishing question

#5

PS

Mark Mandell - Gone Round In Jersey

>Save your 320 and above paper for sanding between coats of finish. Sanding raw wood to 400 is, IMO, a waste of time and effort. I never sand raw wood beyond 220.

Re: finishing question

#6

Re: finishing question

Andy Halterman: Freezing and thawing

>David,

In my flooring business, I use this sealer all the time.

http://www.lastnlast.com/pro/PDabpolFastDry.html#

It's solvent based, but, once dry, you can use waterbased topcoats without worry. I've been doing this for many years and have not had any adhesion problems to speak of. It dries in about 4 hrs under optimal conditions. Figure an overnight dry if used over a minwax stain. Personally, I like it much better than sealcoat which can also raise some grain. Just a personal preference issue more or less.

Hope it helps.

Andy Halterman

No winner in the US vs. Mexico "futbol" bet due to a tie in Hendersonville, NC�

Re: finishing question

#7

150 or 220 drywall sanding screen

Clint Searl, at the base of Haycock Mtn

>

Re: finishing question

#8

Re: finishing problems

Bill Tindall, E.TN

>Agreed, it is not recommended to use steel wool under urethanes but I have done it. But then I dust well with air hose.

I have only one experience with water based urethane floor finish. After coat #1 it was as rough as if I had soaked the wood in water. I ground this roughness off with 220 stearated paper. Next coat went on without difficulty. Results may depend on details of finish formulation, I suppose, especially given that water based finishes do in fact contain appreciable amounts of coalescing solvent of one sort or another.

As far as I know the white stuff is zinc stearate, a soap/surfactant. Many of the water based finishes are synthesized in water with a surfactant. I would not therefore, automatically presume that zinc stearate would cause a problem, but I don't argue with data if someone has shown that it does.

I guess like in all finishing, one should try out the process on a scrap surface.