Just what I found..
Joe Burke
>Clint
I tried the Fuhr products, and while they showed promise, I couldn't ever resolve all the issues I encountered. The consensus among all the experts was that environmental issues are almost always the culprit. In short, the weather.
Here in NC the weather swings so wildly that I couldn't ever get a bead a constant set up. Every time I shot was an adventure.
I really wanted to use the tinted fuhr finishes for my painted work, and did with some success. I've used the clear finishes on drawer boxes and the like, but never liked the look on anything else.
The bottom line was that I needed more consistancy than the water based stuff would give me. I had to go back to the dark side. It doesn't hurt that I have a major distributor for a good solvent based product within 5 miles of the shop either.
I wanted the water based stuff to work in the worst way, but it just wouldn't for me. More power to those that can.