Waterlox Finish Schedule

Doug Reynolds in Seattle

>I posted earlier about finishing a Jatoba cabinet and decided to take Ellis' advice and use Waterlox. I was thinking of applying three coats of their Sealer/Finish, followed by three coats of the High Gloss Finish. How does that sound?

Re: Waterlox Finish Schedule

#2

Ellis Walentine

Reasons for finishing

Ellis Walentine

>Hi Doug,

From your description, it sounds like you want a rather heavy build on this cabinet, possibly heavier than you need. Waterlox gloss builds faster than their sealer because it has more solids in it. It's also not as easy to control with a rag. I've always proceeded with the sealer until I got the depth I wanted, but you can speed up the process with the gloss product.

I'm wondering why you want such a heavy finish on a cabinet? Normally cabinets get little abrasion and handling, except for doors and drawer fronts and tops. Unless you need that extra protection or the depth of the varnish for a particular appearance requirement, I'd normally stick with 4-6 coats of sealer for the cabinet and possibly a couple topcoats of a more abrasion resistant finish for high-wear areas.

Ellis

Re: Waterlox Finish Schedule

#3

Re: Reasons for finishing

Doug Reynolds in Seattle

>Ellis: This is for the jatoba liquor cabinet that will go in a co-worker's vacation condo I wrote about earlier. If three coats of sealer/finish followed by three coats of gloss is too much, lucky me. I am concerned, however, about the top as it will probably get some liquor, water, etc. spilled on it.

Re: Waterlox Finish Schedule

#4

Re: Reasons for finishing

David Yoho

>Doug, Waterlox will protect against those spills. It should be fine.