Re: Actually....
JohnKJordan in East TN
>>reaction wood... Causes fuzzy wood, funny drying, etc.
What's worse, reaction wood can cause severe warping, not only during drying but sometimes sawing releases internal stresses can even warp and crack the boards right on the sawmill.
The smaller logs appear to be limbs of the larger log. I would not buy these with the intention of getting good lumber out of the limbs. (Limbs are great for firewood.) However, some of the crotch wood might provide fantastic turning stock.
BTW, the photo below is from a dead limb which I had to remove from an oak tree here. Notice the similarity to the offset pith in the heart wood on the third and fourth closeup pictures in the ebay link.
This limb was nearly horizontal for at least 40 feet from the tree which explains the extreme reaction wood. The oak tree is about 3' in diameter - I counted nearly 100 growth rings in this limb!
JKJ