1. What is the purpose of the gloss coat between 180/220 and 400 sanding? sealer and begin of thickness build. Gloss for all but the thin top layer gives the finish "depth". Normal procedure.

2. Does the waterlox require spraying? No/ test panels were brushed and it levels wonderfully. I can spray so I do spray. Took about 30 seconds to do the case. 15 seconds per drawer.